查了下维基百科,HPHT法(高温高压)想压出钻石所需的温度和压力和做这表壳的温度压力要求完全不在一个数量级上。。。看来道路还是很曲折滴啊! 如下图制作出的成品体积非常有限,且没有使用任何成型模具的可能: The BARS apparatus is the most compact, efficient, and economical of all the diamond-producing presses. In the center of a BARS device, there is a ceramic cylindrical "synthesis capsule" of about 2 cm3 in size. The cell is placed into a cube of pressure-transmitting material, such as pyrophyllite ceramics, which is pressed by inner anvils made from cemented carbide (e.g., tungsten carbide or VK10 hard alloy).[43] The outer octahedral cavity is pressed by 8 steel outer anvils. After mounting, the whole assembly is locked in a disc-type barrel with a diameter about 1 meter. The barrel is filled with oil, which pressurizes upon heating, and the oil pressure is transferred to the central cell. The synthesis capsule is heated up by a coaxial graphite heater and the temperature is measured with a thermocouple.[44] |
压力和温度都再高点 隔绝活泼气体 直接压出人造钻石表壳 AP加把劲! |
AP的碳壳是这么做出来的? 我还以为是注塑类的方法出来的。真学习了! |
本帖最后由 北无忌 于 2012-8-10 20:16 编辑 我的锻碳,表框/表圈全采用锻碳材料。 |
AP Dial_BJ1.jpg (90.08 KB, 下载次数: 41)
學習了~ |
原来是这样有意思的材料 |
有意思,非常喜欢,就是价格都跟贵金属一样高 |
机械米厉害。 |
AP的皇像啊 |
联系我们|公司简介|隐私政策|手机版|小黑屋|Archiver|名表通 | www.watchlead.com ( 粤ICP备14096658号 )
GMT+8, 2025-2-2 11:21 , Processed in 0.194775 second(s), 44 queries .
Powered by Discuz! X3.2
© 2008-2015 Comsenz Inc.